Electrode Paste - Our Strength:
1. Lower ash content.
2. Acurate dosing and stable volatile content.
3. Good electric and thermal conductivity and the sintering speed appropriate to that of consumption of working end.
4. Smelting at lower temperature with certain fluidity and homogeneous composition.
5. High resistance to high temp, oxidation and thermal shock, low resistivity and high mechanical strength after sintering.
No | Parameter | Specification |
1 | Ash Content | 2 - 10% Max |
2 | Si | 0.28% Max |
3 | Fe | 0.25% Max |
4 | P | 0.00% Max |
5 | V.M | 10.0 - 15.0 |
6 | Density | 1.46 g/cm3 Min |
7 | Compression Strength | 18 Mpa Min |
8 | Resistivity | 55 - 90 uΩm |